Laminator ( self )
submitted 3 years ago by TaylorGang Warning: 0%
Hello fakeid vendors family I have problem with laminating the ids , what's perfect heat degree ? 150c ? and lamination pouches thickness please and what is good laminators in market ?
any help is appreciated please
darkestarke — 3 years ago
10 mil teslin. 7 mil lam in front. 10 in back. Vice versa. Depending on state and sec features on a 3rd over lam ply. Perhaps?
TaylorGang [S] — 3 years ago
appreciate the help bro ... matte laminating right ? 7/10/10
Depends on state… I use glossy…. If needed could use buffer side of nail file. Those big, colorful , 4 sided, 7 textured nail files
plataoplomo — 3 years ago
Ik a good one u can use can u show me where to get the holograms text me tele Bandman1008s
mikesshit — 3 years ago
I could use some guidance on the holos as well have had multiple failed attempts. Please pm me with some answers as well. Thanks
darkestarke —